Product Name: | Insulating Refractory Brick | Material: | Bauxite, Fire Clay, Alumina Powder, Flint Clay |
---|---|---|---|
Shape: | Brick | Al2o3 Content: | 85% |
Application: | Blast Furnace Stove | Bulk Density: | 2.6-2.9g/cm3 |
Type: | Wearing Resistant Refractory Materials | Working Temperature: | 1450℃ |
Standard Size: | 230x114x65mm | OEM ODM: | Acceptable |
High Light: | 230x114x65mm Insulating Refractory Brick,85% Insulating Refractory Brick,230x114x65mm fire resistant bricks |
Blast Furnace Stove 85% 230x114x65mm Insulating Refractory Brick
Insulating Refractory Brick Application:
Feature of Insulating Refractory Brick :
1. Low bulk density, low thermal conductivity, good thermal insulation performance.
2. Refractory category allow direct contact of fire, suitable ofr various atmosphere
3. Good integrity with furnace lining, long service life, easy operation, could be shaped freely
4. Product specification: standard form, normal standard, shaped and special shaped bricks.
5. Can be used in various kilns because of its cheapness and general tray package. Among all of the refractory materials, it is the most widely used.
Specification of Insulating Refractory Brick
Brand Item | Phosphate bonded high alumina bricks | |
HYP-70 | HYPA-80 | |
Al2o3 | 75 | 77 |
Fe2o3 | 3.2 | 3.2 |
Cao | 0.6 | 0.6 |
Bulk Density | 2.65 | 2.70 |
Refractoriness | 1780 | 1780 |
Cold Crushing Strength | 60 | 65 |
0.2 Softening Temperature load Degree T0.6 | 1300 | 1200 |
Thermal conductivity (1000℃)W/M.K |
1.5 | 1.6 |
Details of Insulating Refractory Brick
Classification & Difference
1.Classification
Phosphate brick high alumina bricks are divided into phosphate bricks and phosphate wear bricks.
2.Difference
❉Phosphate brick is used as a binder for phosphate, and phosphate wear-resistant brick is a binder of diammonium phosphate.
❉Generally divided into resistant phosphate and high temperature phosphate. These two bricks are not much different because phosphates have better wear resistance.
❉High-grade phosphate bricks are high-load soft phosphate bricks. Because phosphate bricks are combined with phosphoric acid, the load is generally low. Above 1300 ℃ ~ 1450℃.
Henan HengYu Kiln Refractory Co., Ltd. now mainly produces refractory materials for steel, metallurgy, coking, cement, charcoal, glass and various industrial kiln furnaces. It produces more than 60,000 tons of various stereotyped and amorphous refractory materials annually. The company now owns 45 million fixed assets and 260 employees, including 6 engineers. There are more than 20 engineering and technical personnel, including five departments, six functional departments, three sub-factories, five workshops, one furnace construction engineering team, one R&D center and one testing center.
Contact Person: Mika
Tel: 86-15981951014